Research status of toughening SiC composite ceramics

Wang Wenlong, Chen Gang, Wang Hongjie, Liu Kai   

  1. First author's address: Ningbo Branch of Chinese Academy of Ordnance Science,Ningbo 315000,Zhejiang,China
  • Received:2022-12-21 Online:2024-02-15 Published:2024-02-28

摘要: SiC陶瓷具有优良的性能,被广泛应用于各领域,但因韧性不足而制约其作为结构材料的应用,故提升其韧性已成为研究热点和焦点。因此,综述了颗粒、晶须、纤维和低维纳米材料(碳纳米管和石墨烯)等不同增强相增韧SiC复合陶瓷的研究现状,期望为今后SiC陶瓷的增韧研究提供参考。

关键词: 碳化硅, 陶瓷基复合材料, 颗粒, 晶须, 低维纳米材料

Abstract: SiC ceramics have excellent properties and are widely used in various industries.However,the lack of toughness restricts their application as structural materials.Therefore,improving their toughness has become a research hotspot and focus.The research status of SiC composites toughened by different strengthening phases,such as particle phases,whiskers,fibers and low dimensional nano-materials (carbon nanotubes and graphene),was reviewed,expecting to provide a reference for toughening SiC ceramics in the future.

Key words: silicon carbide, ceramic matrix composites, particle, whisker, low-dimensional nano materials