镁铝尖晶石对煅烧LiNi xCo yMn zO 2正极材料用匣钵材料性能的影响
翟鹏涛, 刘明杨, 周文英, 陈留刚, 丁达飞, 叶国田
Effect of magnesium aluminate spinel on properties of sagger materials for calcining LiNi xCo yMn zO 2 cathode material
Zhai Pengtao, Liu Mingyang, Zhou Wenying, Chen Liugang, Ding Dafei, Ye Guotian
耐火材料 . 2021, (2): 102 -106 .  DOI: 10.3969/j.issn.1001-1935.2021.02.003