升温制度对Al-MgO-Al
2O
3耐火材料物相组成及显微结构的影响
赵臣瑞, 孙洋, 牛智旺, 李勇, 李宏宇, 梁保青
Influence of heating schedule on phase composition and microstructure of Al-MgO-Al
2O
3 refractories
Zhao Chenrui, Sun Yang, Niu Zhiwang, Li Yong, Li Hongyu, Liang Baoqing
耐火材料
.
2021, (2): 107
-110
.
DOI: 10.3969/j.issn.1001-1935.2021.02.004