MgCO
3微粉对刚玉质弥散型透气砖性能的影响
邱鑫, 张仕鸣, 康国卫, 贾全利, 刘新红
Effect of MgCO
3 micropowder on properties of corundum based dispersive purging plugs
Qiu Xin, Zhang Shiming, Kang Guowei, Jia Quanli, Liu Xinhong
耐火材料
.
2021, (3): 190
-193
.
DOI: 10.3969/j.issn.1001-1935.2021.03.002