骨料密度对高纯氧化锆制品性能的影响
谭清华, 孙红刚, 杜一昊, 张涛, 王晗, 闫双志
Effect of aggregate density on properties of high purity zirconia products
Tan Qinghua, Sun Honggang, Du Yihao, Zhang Tao, Wang Han, Yan Shuangzhi
耐火材料 . 2021, (3): 194 -197 .  DOI: 10.3969/j.issn.1001-1935.2021.03.003