利用天然镁橄榄石制备轻质原料的工艺研究及其应用
孟超, 孟庆新, 李晓龙, 蔡翔宇, 高文科, 陈秋阳
Preparation and application of light-weight raw materials from natural forsterite
Meng Chao, Meng Qingxin, Li Xiaolong, Cai Xiangyu, Gao Wenke, Chen Qiuyang
耐火材料 . 2021, (3): 230 -234 .  DOI: 10.3969/j.issn.1001-1935.2021.03.011