大型CFB锅炉高温分离器耐磨砖墙存在问题及改进措施
代泽华, 龚莲辉, 龚兴利, 营利萍, 辛胜伟
Problems and measures of wear-resistant brick wall of high temperature cyclone in a large CFB boiler
Dai Zehua, Gong Lianhui, Gong Xingli, Ying Liping, Xin Shengwei
耐火材料
.
2021, (3): 235
-239
.
DOI: 10.3969/j.issn.1001-1935.2021.03.013