重复使用对纤维增强SiO
2气凝胶材料隔热性能的影响
田响宇, 韩银龙, 周粮, 吴琼, 尚磊, 高庆福, 张博
Effect of repeated usage on thermal insulation properties of fiber reinforced SiO
2 aerogel materials
Tian Xiangyu, Han Yinlong, Zhou Liang, Wu Qiong, Shang Lei, Gao Qingfu, Zhang Bo
耐火材料
.
2021, (2): 116
-120
.
DOI: 10.3969/j.issn.1001-1935.2021.02.006