环氧树脂结合刚玉基多孔陶瓷的制备
刘庆祝, 张佳钰, 孙广超, 司凯凯, 刘开琪, 陈运法
Preparation of corundum-based porous ceramics bonded by epoxy resin
Liu Qingzhu, Zhang Jiayu, Sun Guangchao, Si Kaikai, Liu Kaiqi, Chen Yunfa
耐火材料
.
2021, (1): 13
-16
.
DOI: 10.3969/j.issn.1001-1935.2021.01.003