钢水连续测温传感器Al
2O
3-C管烧制过程温度研究
肖步庆, 孟红记, 李太全, 王峰
Sintering temperature of Al
2O
3-C tubes for continuous temperature sensor of molten steel
Xiao Buqing, Meng Hongji, Li Taiquan, Wang Feng
耐火材料
.
2021, (4): 287
-290
.
DOI: 10.3969/j.issn.1001-1935.2021.04.003