耐火材料抗碱蒸气侵蚀性研究
范沐旭, 侯晓静, 冯志源, 王晗, 刘鹏程, 石干
Alkali vapor corrosion of refractories at high temperatures
Fan Muxu, Hou Xiaojing, Feng Zhiyuan, Wang Han, Liu Pengcheng, Shi Gan
耐火材料 . 2021, (4): 296 -301 .  DOI: 10.3969/j.issn.1001-1935.2021.04.005