氢氧化镁粒度对刚玉-尖晶石材料结构与性能的影响
黄传, 倪月娥, 柯昌明, 刘学新, 王景然, 张锦化
Effect of magnesium hydroxide particle size on structure and properties of corundum-spinel materials
Huang Chuan, Ni Yue’e, Ke Changming, Liu Xuexin, Wang Jingran, Zhang Jinhua
耐火材料
.
2021, (4): 305
-308
.
DOI: 10.3969/j.issn.1001-1935.2021.04.007