MgO和Y 2O 3对气压烧结制备氮化硅陶瓷的影响
余冬玲, 张会玲, 罗宏斌, 冯晓宇, 吴南星
Effects of MgO and Y 2O 3 on preparation of silicon nitride ceramics by gas pressure sintering
Yu Dongling, Zhang Huiling, Luo Hongbin, Feng Xiaoyu, Wu Nanxing
耐火材料 . 2021, (4): 316 -318 .  DOI: 10.3969/j.issn.1001-1935.2021.04.009