发泡-注凝结合催化氮化法制备Si 3N 4多孔陶瓷
韩磊, 李孝建, 张海军
Preparation of Si 3N 4 porous ceramics via foam-gelcasting combined catalytic nitridation
Han Lei, Li Xiaojian, Zhang Haijun
耐火材料 . 2021, (5): 395 -399 .  DOI: 10.3969/j.issn.1001-1935.2021.05.005