Al粉、Si粉复合低碳稳定镁钙材料的抗氧化性
高正霞, 陶梦雅, 刘伟, 孟维, 马成良, 钟香崇
Oxidation resistance of Al/Si composite low-carbon stabilized MgO-CaO materials
Gao Zhengxia, Tao Mengya, Liu Wei, Meng Wei, Ma Chengliang, Zhong Xiangchong
耐火材料
.
2021, (5): 430
-434
.
DOI: 10.3969/j.issn.1001-1935.2021.05.012