β-SiAlON含量对SiAlON结合刚玉材料性能的影响
刘晨晖, 张宇翠, 贾全利, 叶方保, 钟香崇
Effect of β-SiAlON content on properties of SiAlON bonded corundum materials
Liu Chenhui, Zhang Yucui, Jia Quanli, Ye Fangbao, Zhong Xiangchong
耐火材料 . 2021, (5): 452 -455 .  DOI: 10.3969/j.issn.1001-1935.2021.05.017