MgCO
3微粉加入量对氧化铝空心球浇注料结构和性能的影响
胡书禾, 陈留刚, 李飞, 田学坤, 张阳, 叶国田
Effect of MgCO
3 micro-powder addition on structure and properties of alumina bubble castables
Hu Shuhe, Chen Liugang, Li Fei, Tian Xuekun, Zhang Yang, Ye Guotian
耐火材料
.
2021, (5): 456
-460
.
DOI: 10.3969/j.issn.1001-1935.2021.05.018