Fe、Co及Ni单掺3C-SiC力学性能的第一性原理计算
闪静祎, 黄珍霞, 王军凯, 李韬, 周轩, 邢盈盈
First-principles calculation of mechanical properties of Fe,Co and Ni doped 3C-SiC
Shan Jingyi, Huang Zhenxia, Wang Junkai, Li Tao, Zhou Xuan, Xing Yingying
耐火材料
.
2021, (6): 476
-482
.
DOI: 10.3969/j.issn.1001-1935.2021.06.004