铝酸钙水泥种类对Al
2O
3-SiC-C质铁沟浇注料性能的影响
牛春林, 任林, 张晓波
Effect of different calcium aluminate cements on properties of Al
2O
3-SiC-C iron trough castables
Niu Chunlin, Ren Lin, Zhang Xiaobo
耐火材料
.
2021, (6): 483
-486
.
DOI: 10.3969/j.issn.1001-1935.2021.06.005