保温时间对SiC-TiC复合粉末物相组成和显微结构的影响
刘鑫, 胡继林, 朱凌, 田修营, 彭秧锡
Effect of holding time on phase composition and microstructure of SiC-TiC composite powder
Liu Xin, Hu Jilin, Zhu Ling, Tian Xiuying, Peng Yangxi
耐火材料 . 2021, (6): 487 -490 .  DOI: 10.3969/j.issn.1001-1935.2021.06.006