高碳铬铁渣制备镁橄榄石-尖晶石复相材料的性能研究
冯泽成, 赵惠忠, 韩欢师, 李轶翀, 马九宏, 杨阳
Properties of forsterite-spinel composite materials prepared by high-carbon ferrochrome slag
Feng Ze-cheng, Zhao Huizhong, Han Huanshi, Li Yichong, Ma Jiuhong, Yang Yang
耐火材料 . 2021, (6): 491 -497 .  DOI: 10.3969/j.issn.1001-1935.2021.06.007