煅烧温度对莫来石质多孔陶瓷材料性能的影响
胡其国, 王明华, 邵晴, 李济, 李小龙
Effect of calcination temperature on properties of porous mullite ceramic materials
Hu Qiguo, Wang Minghua, Shao Qing, Li Ji, Li Xiaolong
耐火材料 . 2021, (6): 502 -504 .  DOI: 10.3969/j.issn.1001-1935.2021.06.009