干熄焦旋转焦罐用莫来石质复合衬板的应用
徐国涛, 盛军波, 冯强, 涂红兵, 王大春, 刘黎, 张燕伟, 张洪雷
Application of mullite composite lining plates for dry quenching rotary coke tanks
Xu Guotao, Sheng Junbo, Feng Qiang, Tu Hongbing, Wang Dachun, Liu Li, Zhang Yanwei, Zhang Honglei
耐火材料
.
2021, (6): 514
-516
.
DOI: 10.3969/j.issn.1001-1935.2021.06.012