添加浮选镁砂颗粒和Al 2O 3细粉对方镁石-尖晶石砖性能的影响
李燕京, 孙加林, 李勇, 康剑, 马淑龙, 马飞, 高长贺, 张积礼, 张海波
Effect of flotation magnesia particles and Al 2O 3 fines on properties of periclase-spinel bricks
Li Yanjing, Sun Jialin, Li Yong, Kang Jian, Ma Shulong, Ma Fei, Gao Changhe, Zhang Jili, Zhang Haibo
耐火材料 . 2022, (1): 6 -9 .  DOI: 10.3969/j.issn.1001-1935.2022.01.002