5.42 m
3梭式窑窑体内衬材料节能效果的有限元分析和优化配置
孟超, 王鹏灿, 杨文刚, 孟庆新, 许佳佳
Finite element analysis on energy saving effect of lining materials of a 5.42 m
3 shuttle kiln body and their optimal configuration
Meng Chao, Wang Pengcan, Yang Wengang, Meng Qingxin, Xu Jiajia
耐火材料
.
2022, (1): 65
-70
.