热处理温度对低硅含量SiO
2微粉固废性能的影响
卫迎锋, 占华生, 田江涛, 陈绍鑫, 叶大俊, 王玉存, 高长贺
Effect of heat treatment temperature on performance of low-silica SiO
2 micropowder solid waste
Wei Yingfeng, Zhan Huasheng, Tian Jiangtao, Chen Shaoxin, Ye Dajun, Wang Yucun, Gao Changhe
耐火材料
.
2022, (1): 71
-74
.
DOI: 10.3969/j.issn.1001-1935.2022.01.016