反应烧结碳化硅高温性能的研究进展
董博, 余超, 邓承继, 祝洪喜, 丁军, 朱青友
Research progress on hot performance of reaction sintered silicon carbide
Dong Bo, Yu Chao, Deng Chengji, Zhu Hongxi, Ding Jun, Zhu Qingyou
耐火材料
.
2022, (1): 75
-81
.
DOI: 10.3969/j.issn.1001-1935.2022.01.017