H2O2加入量对ρ-Al2O3结合刚玉浇注料抗爆裂性能的影响
王欢, 王战民, 冯海霞, 曹迎楠, 柳军, 许应顺
Effect of H 2O 2 addition on anti-explosion performance of ρ-Al 2O 3 bonded corundum castables
Wang Huan, Wang Zhanmin, Feng Haixia, Cao Yingnan, Liu Jun, Xu Yingshun
耐火材料 . 2022, (2): 107 -111 .  DOI: 10.3969/j.issn.1001-1935.2022.02.003