TiO
2加入量对光固化打印成型Al
2O
3陶瓷性能的影响
王瑞, 杨道媛, 原会雨, 崔俊艳
Effect of TiO
2 addition on properties of Al
2O
3 ceramics prepared by digital light printing (DLP)
Wang Rui, Yang Daoyuan, Yuan Huiyu, Cui Junyan
耐火材料
.
2022, (2): 112
-116
.