黏结剂种类对铝酸镧涂层材料性能的影响
张一帆, 王曲, 王刚, 刘鹏程, 张琪, 司瑶晨
Effect of binder types on properties of lanthanum aluminate coating materials
Zhang Yifan, Wang Qu, Wang Gang, Liu Pengcheng, Zhang Qi, Si Yaochen
耐火材料
.
2022, (2): 123
-126
.
DOI: 10.3969/j.issn.1001-1935.2022.02.006