氧化铝微粉的特性和分散剂对浆料流变特性的影响
石颖恒, 王超, 员文杰
Effects of alumina micro-powder characteristics and dispersants on rheological properties of alumina slu-rries
Shi Yingheng, Wang Chao, Yuan Wenjie
耐火材料
.
2021, (1): 21
-25
.
DOI: 10.3969/j.issn.1001-1935.2021.01.005