基于第一性原理计算的石墨氧化机制探讨
毕玉保, 王慧芳, 张海军
Discussion on oxidation mechanism of graphite based on First Principle calculation
Bi Yubao, Wang Huifang, Zhang Haijun
耐火材料 . 2022, (3): 202 -205 .  DOI: 10.3969/j.issn.1001-1935.2022.03.005