脉冲电场对浸入式水口渣线耐火材料侵蚀的影响
李延, 袁磊, 田晨, 刘国齐, 于景坤, 李红霞
Effect of pulsed electric field on corrosion of slag line refractories for submerged entry nozzles
Li Yan, Yuan Lei, Tian Chen, Liu Guoqi, Yu Jingkun, Li Hongxia
耐火材料 . 2022, (5): 374 -379 .  DOI: 10.3969/j.issn.1001-1935.2022.05.002