SiO 2微粉添加量对刚玉浇注料抗热震性的影响
李玉川, 张三华, 秦红彬, 陈卢
Effect of SiO 2 fume addition on thermal shock resistance of corundum castables
Li Yuchuan, Zhang Sanhua, Qin Hongbin, Chen Lu
耐火材料 . 2022, (5): 407 -411 .  DOI: 10.3969/j.issn.1001-1935.2022.05.008