碳化硼材料的烧结致密化及其应用研究进展
邹鑫, 陈平安, 徐广平, 李享成, 朱颖丽, 朱伯铨
Sintering densification of boron carbide materials and their application research progress
Zou Xin, Chen Ping’an, Xu Guangping, Li Xiangcheng, Zhu Yingli, Zhu Boquan
耐火材料
.
2022, (5): 452
-457
.
DOI: 10.3969/j.issn.1001-1935.2022.05.018