燃气轮机燃烧室用陶瓷瓦块的定量无损检测方法研究
冯志源, 王晗, 宋艳艳, 范沐旭, 张涛, 武刚
Quantitative non-destructive testing method of ceramic tiles for gas turbine combustors
Feng Zhiyuan, Wang Han, Song Yanyan, Fan Muxu, Zhang Tao, Wu Gang
耐火材料 . 2022, (5): 458 -460 .  DOI: 10.3969/j.issn.1001-1935.2022.05.019