催化剂对Al
2O
3-SiC-C浇注料显微结构和性能的影响
程翠丽, 赵子尖, 任世怡, 李磊, 陈平安, 李享成, 朱伯铨
Effects of catalyst on microstructure and properties of Al
2O
3-SiC-C castables
Cheng Cuili, Zhao Zijian, Ren Shiyi, Li Lei, Chen Ping'an, Li Xiangcheng, Zhu Boquan
耐火材料
.
2022, (4): 320
-324
.
DOI: 10.3969/j.issn.1001-1935.2022.04.010