B 4C加入量对硅溶胶结合莫来石-刚玉浇注料性能的影响
蔡玮, 陈金凤, 鞠茂奇, 丛培源
Effect of B 4C addition on properties of silica sol bonded mullite-corundum castables
Cai Wei, Chen Jinfeng, Ju Maoqi, Cong Peiyuan
耐火材料 . 2022, (4): 325 -328 .  DOI: 10.3969/j.issn.1001-1935.2022.04.011