氧化锆添加量对镁质材料性能的影响
高永军, 吴锋, 李心慰, 苏玉玺, 冯雨罗旭东, 陈卫敏, 王琼
Effect of zirconia addition on properties of magnesia refractories
Gao Yongjun, Wu Feng, Li Xinwei, Su Yuxi, Feng Yu, Luo Xudong, Chen Weimin, Wang Qiong
耐火材料
.
2022, (4): 339
-341
.
DOI: 10.3969/j.issn.1001-1935.2022.04.014