SiO
2粒度和反应温度对熔盐法合成莫来石晶须的影响
苏玉玺, 李心慰, 吴锋, 高永军, 罗旭东, 冯雨, 陈卫敏
Effect of SiO
2 particle size and reaction temperature on synthesis of mullite whiskers by molten salt method
Su Yuxi, Li Xinwei, Wu Feng, Gao Yongjun, Luo Xudong, Feng Yu, Chen Weimin
耐火材料
.
2022, (4): 342
-345
.
DOI: 10.3969/j.issn.1001-1935.2022.04.015