硝酸铁负载方式对氮化制备Si 3N 4复合MgO-C材料的影响
陈洋, 邓承继, 丁军, 余超, 娄晓明
Effect of ferric nitrate loading mode on properties of Si 3N 4 composite MgO-C refractories prepared by nitridation
Chen Yang, Deng Chengji, Ding Jun, Yu Chao, Lou Xiaoming
耐火材料 . 2022, (6): 477 -480 .  DOI: 10.3969/j.issn.1001-1935.2022.06.004