富铝尖晶石微粉对刚玉-尖晶石浇注料关键使用性能的影响
肖雄, 魏耀武, 周辉, 颜林, 陈志强, 邵长波
Influence of alumina-rich spinel micropowder on key performances of corundum-spinel castables
Xiao Xiong, Wei Yaowu, Zhou Hui, Yan Lin, Chen Zhiqiang, Shao Changbo
耐火材料
.
2022, (6): 499
-504
.
DOI: 10.3969/j.issn.1001-1935.2022.06.009