尖晶石微粉对铝镁质干式捣打料性能的影响
姜广森, 聂建华, 李洪波, 梁永和, 蔡曼菲
Influence of spinel micropowder on properties of alumina-magnesia dry ramming mixes
Jiang Guangsen, Nie Jianhua, Li Hongbo, Liang Yonghe, Cai Manfei
耐火材料 . 2022, (6): 539 -542 .  DOI: 10.3969/j.issn.1001-1935.2022.06.018