熔融沉积法3D打印制备多孔氧化锆陶瓷
牛富荣, 张力, 郭金玉, 刘鹏, 杨现锋, 谢志鹏
Preparation of porous zirconia ceramics by fused deposition 3D printing
Niu Furong, Zhang Li, Guo Jinyu, Liu Peng, Yang Xianfeng, Xie Zhipeng
耐火材料 . 2023, (1): 20 -26 .  DOI: 10.3969/j.issn.1001-1935.2023.01.005