熔盐法合成α-Si
3N
4-AlN复合粉体及其抗水化性能
王森, 梁峰, 王晓函, 谷昊辉, 吴帅兵, 吕功业, 张海军
Synthesis and hydration resistance of α-Si
3N
4-AlN composite powder by molten salt method
Wang Sen, Liang Feng, Wang Xiaohan, Gu Haohui, Wu Shuaibing, Lyu Gongye, Zhang Haijun
耐火材料
.
2023, (1): 27
-30
.
DOI: 10.3969/j.issn.1001-1935.2023.01.006