用石油焦后玻璃窑碱性耐火材料侵蚀及对策
王杰曾, 刘昭, 徐琳琳, 陈松林, 刘锡俊
Corrosion of basic refractories for glass tanks using petrol coke and countermeasures
Wang Jiezeng, Liu Zhao, Xu Linlin, Chen Songlin, Liu Xijun
耐火材料 . 2023, (1): 50 -54 .  DOI: 10.3969/j.issn.1001-1935.2023.01.011