煅烧温度对菱镁矿尾矿制备MgO-MgAl
2O
4-Mg
2SiO
4复相多孔材料性能的影响
周萍, 马北越, 任鑫明
Effect of calcination temperature on properties of MgO-MgAl
2O
4-Mg
2SiO
4 complex porous materials prepared from magnesite tailings
Zhou Ping, Ma Beiyue, Ren Xinming
耐火材料
.
2023, (2): 104
-106
.
DOI: 10.3969/j.issn.1001-1935.2023.02.003