匣钵材料抗氢氧化锂侵蚀性研究
郑翰, 马昭阳, 曹会彦, 万龙刚, 相宇博, 钱凡, 吴吉光
Lithium hydroxide corrosion resistance of three sagger materials
Zheng Han, Ma Zhaoyang, Cao Huiyan, Wan Longgang, Xiang Yubo, Qian Fan, Wu Jiguang
耐火材料 . 2023, (2): 125 -130 .  DOI: 10.3969/j.issn.1001-1935.2023.02.008