不同粒度锌铝尖晶石加入量对方镁石-锌铝尖晶石性能的影响
谢永涣, 田琳, 毛硕, 马淑龙, 吴师岗, 李国华
Effect of different particle sizes zinc alumina spinel addition on properties of periclase-zinc alumina spinel
Xie Yonghuan, Tian Lin, Mao Shuo, Ma Shulong, Wu Shigang, Li Guohua
耐火材料 . 2023, (2): 149 -152 .  DOI: 10.3969/j.issn.1001-1935.2023.02.013