烧成温度对钛基铝酸盐水泥性能的影响
张康康, 马淑龙, 苏玉柱, 杨晨, 刘磊, 李燕京, 罗华明
Effect of firing temperature on properties of titanium-based aluminate cement
Zhang Kangkang, Ma Shulong, Su Yuzhu, Yang Chen, Liu Lei, Li Yanjing, Luo Huaming
耐火材料 . 2023, (2): 166 -168 .  DOI: 10.3969/j.issn.1001-1935.2023.02.017